Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 63.54 MPa @Strain 4.42 %, Temperature 150 °C |
9216 psi @Strain 4.42 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |