Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 92.16 MPa @Strain 2.56 %, Temperature 23.0 °C |
13370 psi @Strain 2.56 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |