Polymer Property : Tensile Stress = 9076 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 62.58 MPa

@Strain 1.99 %,
Temperature 90.0 °C
9076 psi

@Strain 1.99 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..
Tensile Stress 62.58 MPa

@Strain 0.730 %,
Temperature 23.0 °C
9076 psi

@Strain 0.730 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..