Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 62.48 MPa @Strain 3.89 %, Temperature 90.0 °C |
9062 psi @Strain 3.89 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |