Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.87 MPa @Strain 0.200 %, Temperature 150 °C |
1430 psi @Strain 0.200 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Stress | 9.87 MPa @Strain 171.75 %, Temperature 150 °C |
1430 psi @Strain 171.75 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |