Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.41 MPa @Strain 88.18 %, Temperature 120 °C |
1360 psi @Strain 88.18 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 9.41 MPa @Strain 88.18 %, Temperature 120 °C |
1360 psi @Strain 88.18 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |