Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 88.6 MPa @Strain 2.92 %, Temperature 23.0 °C |
12900 psi @Strain 2.92 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |