Polymer Property : Tensile Stress = 877 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.05 MPa

@Strain 100 %
877 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F02-138A TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..