Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 87.3 MPa @Strain 4.00 %, Temperature -40.0 °C |
12700 psi @Strain 4.00 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |