Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 59.13 MPa @Strain 5.77 %, Temperature 0.000 °C |
8576 psi @Strain 5.77 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |