Mechanical Properties Metric English Comments
Tensile Stress 58.28 MPa

@Strain 3.57 %,
Temperature 150 °C
8453 psi

@Strain 3.57 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66  (Unverified Data**)
33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin..
Tensile Stress 58.28 MPa

@Strain 0.400 %,
Temperature 23.0 °C
8453 psi

@Strain 0.400 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 51G45HSL NC010 Polyphthalamide (PPA)  (Unverified Data**)
45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL NC010 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information ..