Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.83 MPa @Strain 100 % |
845 psi @Strain 100 % |
ASTM D1708 |
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |