Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 83.07 MPa @Strain 5.65 %, Temperature -40.0 °C |
12050 psi @Strain 5.65 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |