Polymer Property : Tensile Stress = 8286 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 57.13 MPa

@Strain 1.69 %,
Temperature 180 °C
8286 psi

@Strain 1.69 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66  (Unverified Data**)
43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 57.13 MPa

@Strain 0.520 %,
Temperature 60.0 °C
8286 psi

@Strain 0.520 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..