Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 55.4 MPa @Strain 1.44 %, Temperature 40.0 °C |
8040 psi @Strain 1.44 %, Temperature 104 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 55.4 MPa @Strain 40.0 %, Temperature 23.0 °C |
8040 psi @Strain 40.0 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |