Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.16 MPa @Strain 300 %, Temperature 23.0 °C |
1180 psi @Strain 300 %, Temperature 73.4 °F |
Die C Across Flow 2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |