Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | >= 8.094 MPa @Strain 50.0 % |
>= 1174 psi @Strain 50.0 % |
ASTM D412 Method A |
Seals Eastern 5795 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |