Mechanical Properties Metric English Comments
Tensile Stress 54.28 MPa

@Strain 0.980 %,
Temperature 40.0 °C
7873 psi

@Strain 0.980 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..