Polymer Property : Tensile Stress = 78.99 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 78.99 MPa

@Strain 1.80 %,
Temperature 150 °C
11460 psi

@Strain 1.80 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..