Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 78.81 MPa @Strain 1.25 %, Temperature 23.0 °C |
11430 psi @Strain 1.25 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |