Polymer Property : Tensile Stress = 7697 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 53.07 MPa

@Strain 1.26 %,
Temperature 120 °C
7697 psi

@Strain 1.26 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Crastin® SK609 NC010 PBT  (Unverified Data**)
Crastin® SK609 NC010 is a 50% glass fiber reinforced, lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers