Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.19 MPa @Strain 300 % |
753 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-137D TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 5.19 MPa @Strain 0.0300 %, Temperature 40.0 °C |
753 psi @Strain 0.0300 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |