Tensile Stress 51.91 MPa

@Strain 0.780 %,
Temperature 23.0 °C
7529 psi

@Strain 0.780 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
Tensile Stress 51.91 MPa

@Strain 1.51 %,
Temperature 90.0 °C
7529 psi

@Strain 1.51 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66  (Unverified Data**)
40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I..