Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 74.54 MPa @Strain 6.66 %, Temperature -20.0 °C |
10810 psi @Strain 6.66 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |