Mechanical Properties Metric English Comments
Tensile Stress 50.4 MPa

@Thickness 0.0500 mm
7310 psi

@Thickness 0.00197 in
TD, Break; ASTM D882
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC)
TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be..
Tensile Stress 50.4 MPa

@Strain 0.800 %,
Temperature -40.0 °C
7310 psi

@Strain 0.800 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66  (Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan..