Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 49.8 MPa @Strain 0.500 %, Temperature 23.0 °C |
7220 psi @Strain 0.500 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 49.8 MPa @Strain 0.680 %, Temperature 23.0 °C |
7220 psi @Strain 0.680 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |