Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.94 MPa @Strain 64.68 %, Temperature 90.0 °C |
716 psi @Strain 64.68 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 4.94 MPa @Strain 6.00 %, Temperature 40.0 °C |
716 psi @Strain 6.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |