Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.87 MPa @Strain 24.3 %, Temperature 40.0 °C |
1140 psi @Strain 24.3 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |