Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.86 MPa @Strain 300 %, Temperature 23.0 °C |
1140 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo.. |
|||
Tensile Stress | 7.86 MPa @Strain 300 %, Temperature 23.0 °C |
1140 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Tensile Stress | 7.86 MPa @Strain 174.81 %, Temperature 120 °C |
1140 psi @Strain 174.81 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |