Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.84 MPa @Strain 173.61 %, Temperature 120 °C |
1140 psi @Strain 173.61 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |