Tensile Stress | 7.80 MPa @Strain 5.00 % |
1130 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tensile Stress | 7.80 MPa @Strain 0.600 %, Temperature 80.0 °C |
1130 psi @Strain 0.600 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 7.80 MPa @Strain 11.79 %, Temperature 120 °C |
1130 psi @Strain 11.79 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.80 MPa @Strain 5.00 % |
1130 psi @Strain 5.00 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |