Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.73 MPa @Strain 0.0900 %, Temperature -20.0 °C |
1120 psi @Strain 0.0900 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 7.73 MPa @Strain 87.01 %, Temperature 120 °C |
1120 psi @Strain 87.01 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.73 MPa @Strain 116.86 %, Temperature 160 °C |
1120 psi @Strain 116.86 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 7.73 MPa @Strain 28.06 %, Temperature 120 °C |
1120 psi @Strain 28.06 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.73 MPa @Strain 116.86 %, Temperature 160 °C |
1120 psi @Strain 116.86 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |