Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.55 MPa @Strain 4.24 %, Temperature 150 °C |
1100 psi @Strain 4.24 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 7.55 MPa @Strain 26.45 %, Temperature 60.0 °C |
1100 psi @Strain 26.45 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.55 MPa @Strain 40.03 %, Temperature 120 °C |
1100 psi @Strain 40.03 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 7.55 MPa @Strain 82.79 %, Temperature 150 °C |
1100 psi @Strain 82.79 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.55 MPa @Strain 40.03 %, Temperature 120 °C |
1100 psi @Strain 40.03 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.55 MPa @Strain 0.600 %, Temperature 90.0 °C |
1100 psi @Strain 0.600 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M40 NC010 Nylon 6
(Unverified Data**) 40% Mineral Reinforced Polyamide 6 Minlon 73M40 NC010 is a 40% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |