Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.29 MPa @Strain 1.30 %, Temperature 40.0 °C |
1060 psi @Strain 1.30 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |