Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.11 MPa @Strain 0.180 %, Temperature 180 °C |
1030 psi @Strain 0.180 %, Temperature 356 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66
(Unverified Data**) Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in.. |
|||
Tensile Stress | 7.11 MPa @Strain 133.72 %, Temperature 120 °C |
1030 psi @Strain 133.72 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |