Mechanical Properties Metric English Comments
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P1790 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ EG-9090 Thermoplastic Elastomer (TPE)
The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun..
Tensile Stress 7.03 MPa

@Strain 100 %
1020 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® D6785 TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress 7.03 MPa

@Strain 3.09 %,
Temperature 90.0 °C
1020 psi

@Strain 3.09 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide..
Tensile Stress 7.03 MPa

@Strain 111.25 %,
Temperature 120 °C
1020 psi

@Strain 111.25 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 7.03 MPa

@Strain 138.82 %,
Temperature 120 °C
1020 psi

@Strain 138.82 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress 7.03 MPa

@Strain 100 %
1020 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer
Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer
Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan..
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 7.03 MPa

@Strain 300 %
1020 psi

@Strain 300 %
ASTM D412
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..