Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 69.79 MPa @Strain 1.38 %, Temperature 23.0 °C |
10120 psi @Strain 1.38 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |