Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 46.09 MPa @Strain 0.790 %, Temperature -20.0 °C |
6685 psi @Strain 0.790 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 46.09 MPa @Strain 0.790 %, Temperature -20.0 °C |
6685 psi @Strain 0.790 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene.. |
|||
Tensile Stress | 46.09 MPa @Strain 3.43 %, Temperature 150 °C |
6685 psi @Strain 3.43 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 540SUV BK544 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass Reinforced UV Stabilized Polyethylene Terephthalate Developed for Extrusion and Injection Molding Rynite 540SUV BK544 is a 40% glass fiber reinforced UV stabilized modified polyethylene te.. |
|||
Tensile Stress | 46.09 MPa @Strain 0.480 %, Temperature 0.000 °C |
6685 psi @Strain 0.480 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) 40% Glass/Mineral Reinforced Polyamide 66 Zytel FE270038 is a 40% glass fiber/mineral reinforced heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.I.. |
|||
Tensile Stress | 46.09 MPa @Strain 20.01 %, Temperature 40.0 °C |
6685 psi @Strain 20.01 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |