Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 45.92 MPa @Strain 0.760 %, Temperature 23.0 °C |
6660 psi @Strain 0.760 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 45.9 MPa @Strain 1.10 %, Temperature 90.0 °C |
6660 psi @Strain 1.10 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |