Mechanical Properties Metric English Comments
Tensile Stress 4.31 MPa

@Strain 31.01 %,
Temperature 120 °C
625 psi

@Strain 31.01 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Tensile Stress 4.31 MPa

@Strain 14.09 %,
Temperature 90.0 °C
625 psi

@Strain 14.09 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..