Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.430 MPa @Strain 0.0200 %, Temperature -40.0 °C |
62.4 psi @Strain 0.0200 %, Temperature -40.0 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 0.430 MPa @Strain 0.0400 %, Temperature 60.0 °C |
62.4 psi @Strain 0.0400 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |