Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 62.15 MPa @Strain 1.90 %, Temperature 90.0 °C |
9014 psi @Strain 1.90 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |