Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 42.3 MPa @Strain 1.40 %, Temperature 23.0 °C |
6140 psi @Strain 1.40 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |