Tensile Stress 61.33 MPa

@Strain 2.53 %,
Temperature 90.0 °C
8895 psi

@Strain 2.53 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
Tensile Stress 61.33 MPa

@Strain 4.24 %,
Temperature 23.0 °C
8895 psi

@Strain 4.24 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers