Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 6060 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 41.8 MPa

@Strain 1.50 %,
Temperature 0.000 °C
6060 psi

@Strain 1.50 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)  (Unverified Data**)
Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr..
Tensile Stress 41.8 MPa

@Strain 0.830 %,
Temperature 120 °C
6060 psi

@Strain 0.830 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Rynite® FR543 NC010 PET
Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm..
Copyright © lookpolymers.com All Rights Reserved