Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 60.5 MPa @Strain 3.36 %, Temperature 40.0 °C |
8770 psi @Strain 3.36 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |