Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 6.80 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.80 MPa

@Strain 50.0 %,
Temperature 23.0 °C
986 psi

@Strain 50.0 %,
Temperature 73.4 °F
ISO 527 (1BA bar)
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET  (Unverified Data**)
Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a..
Tensile Stress 6.80 MPa

@Strain 85.36 %,
Temperature 160 °C
986 psi

@Strain 85.36 %,
Temperature 320 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 6.80 MPa

@Strain 85.36 %,
Temperature 160 °C
986 psi

@Strain 85.36 %,
Temperature 320 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers