Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 6.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.50 MPa

@Strain 26.33 %,
Temperature 150 °C
943 psi

@Strain 26.33 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 6.50 MPa

@Strain 28.27 %,
Temperature 90.0 °C
943 psi

@Strain 28.27 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET  (Unverified Data**)
47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 6.50 MPa

@Strain 15.83 %,
Temperature 100 °C
943 psi

@Strain 15.83 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me..
Tensile Stress 6.50 MPa

@Strain 41.29 %,
Temperature 90.0 °C
943 psi

@Strain 41.29 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 6.50 MPa

@Strain 50.0 %
943 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® RS 40F3 NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Renewably Sourced High Flow Polyester Elastomer Developed for Injection Molding Hytrel RS 40F3 NC010 is a high flow low modulus grade containing at least 50% renewably sourced ingredients..
Tensile Stress 6.50 MPa

@Strain 15.83 %,
Temperature 100 °C
943 psi

@Strain 15.83 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET
55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers
Tensile Stress >= 6.50 MPa

@Strain 100 %
>= 943 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 485A Polyester-based TPU
Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Tensile Stress >= 6.50 MPa

@Strain 100 %
>= 943 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 790A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Copyright © lookpolymers.com All Rights Reserved