Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.38 MPa @Strain 6.97 %, Temperature 100 °C |
925 psi @Strain 6.97 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |