Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 6.07 MPa

@Strain 300 %
880 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2085 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..